Why don't you try sprinkling a layer of the crystals on a pad made from a
wet paper towel and wiping the hot iron tip across it? Try dampening the
crystals just slightly (spritz with a spray bottle?)

My SalAmmoniac block gives off "grit" when I use it, sometimes I catch that
grit and put it on a wet sponge in the iron holder. It adds just enough
"abrasive" with the sponge to keep the tip just right.